A Raman Spectroscopic Study of MoS2 and MoO3: Applications to Tribological Systems
By B. Windom, W. Gregory Sawyer, D. Hahn. 2011
673 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanical Engineering, Mechanics of Materials
View Paper: https://www.semanticscholar.org/paper/6d9dfbe26d51d14bcd96ec568b6876bfcea07035
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
- Zhangting Wu
- Lain‐Jong Li
- Zhenhua Ni
- Gurpreet Singh
- Mohammad R. Vazirisereshk
- H. Spikes
- Ashlie Martini
- David A. Strubbe
In Mechanical Engineering
- Mehmet Baykara
- Ashlie Martini
- Mohammad R. Vazirisereshk
- David A. Strubbe
- Lain‐Jong Li
- D. Burris
- Zhenhua Ni
- H. Spikes
In Mechanics of Materials
- Mehmet Baykara
- Ashlie Martini
- David A. Strubbe
- Mohammad R. Vazirisereshk
- H. S. Khare
- D. Burris
- H. Spikes
- W. Gregory Sawyer
Citations in the corpus
- From two-dimensional materials to their heterostructures: An electrochemist's perspective (2017, background): “The Raman spectra of group 6 semiconducting TMDCs show additional resonant modes, which appear when the excitation energy is close to the direct band gap transitions at the K (K′) point [29,133,157,160].”
- Few-Layer MoS2 with high broadband Photogain and fast optical switching for use in harsh environments. (2013, background): “It should be noted that the oxidation of MoS2 to MoO3 in a dry O2 environment could occur at 375 K.(52) Moreover, Mikheev et al.”
- Friction Modifier Additives (2015, methodology): “XPS and Raman have subsequently become widely used tools to study organomolybdenum additive tribofilms [144, 145].”
- Solid Lubrication with MoS2: A Review (2019, methodology): “The transition temperature at which the oxidation rate increases substantially has been reported to be from 100 oC [109,110] to 400 oC [111,112], which may depend strongly on the preparation method of the MoS2 film and on film conditioning induced by deliberate thermal cycling during sliding prior t”
- The Effects of Environmental Water and Oxygen on the Temperature-Dependent Friction of Sputtered Molybdenum Disulfide (2013, background): “and oxidation studies report that oxidation only occurs above a transition temperature that ranges from 100 to 500 C [1, 3, 24, 25, 27, 28]; Windom et al.”
- Spectroscopic investigation of defects in two-dimensional materials (2016, background): “After air heating at 400 °C, two peaks at 695 and 803 cm −1 are observed for few-layer WSe2 sample, which are assigned to tungsten oxide (WO3-x) [113].”