Mechanical properties of spruce wood cell walls by nanoindentation
By W. Gindl, H. Gupta, T. Schöberl, Helga C. Lichtenegger, P. Fratzl. 2004
277 citations recorded by the source corpus.
Subfields: Biomaterials, Biomedical Engineering, Building and Construction
View Paper: https://www.semanticscholar.org/paper/e7ec3b09d6b77669321afa3bccc968afb38a57c9
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomaterials
In Biomedical Engineering
In Building and Construction
Citations in the corpus
- Nanoindentation of wood cell walls: Continuous stiffness and hardness measurements (2007, unknown): “[24].”
- Conversion of Lignocellulosic Biomass to Nanocellulose: Structure and Chemical Process (2014, background): “The presence of cellulose in biomass is able to depolymerise into nanodimension biomaterial, with exceptional mechanical properties for biocomposites, pharmaceutical carriers, and electronic substrate’s application.”
- Microfibril Angle: Measurement, Variation and Relationships – A Review (2008, background): “Using nano-indentation of cell wall regions, Gindl et al. (2004) con-”
- Quantitative trait locus (QTL) analysis of wood quality traits in Eucalyptus nitens (2010, background): “A number of studies have shown positive relationships between MFA and lignin content (Gindl et al. 2004; Gindl and Teischinger 2002; Hori et al. 2003).”
- Mechanical characterization of single bamboo fibers with nanoindentation and microtensile technique (2010, methodology): “The subsequent investigations conducted by Gindl and Gupta (2002a) and Gindl et al. (2004) focused on microfibril angle (MFA) and lignification related to longitudinal hardness and elastic modulus of the secondary cell wall of softwood tracheids.”
- ADHESIVE PENETRATION IN WOOD—A REVIEW (2007, background): “The effect of resin impregnation, independent of adhesive bonding, on the mechanical properties of wood has been investigated (Furuno et al. 2004; Miroy et al. 1995; Gindl and Gupta 2002; Gindl et al. 2004; Nakata et al. 1997; Shams et al. 2004).”
- Mechanics of balsa (Ochroma pyramidale) wood (2015, background): “These values are mostly in agreement with the 0.40-0.56 GPa for hardness and 16-24 GPa for reduced modulus reported for 10 different hardwoods (Wu et al. 2009) and for spruce wood tracheids with mean MFAs close to 0° (Gindl et al. 2004).”