Crystallographic fatigue crack initiation in nickel-based superalloy René 88DT at elevated temperature
By J. Miao, Tresa M. Pollock, J. Jones. 2009
311 citations recorded by the source corpus.
Subfields: Mechanical Engineering, Mechanics of Materials, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/a407223d37a4ae5bef25cae6c0ab0b56d86b7f5a
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Mechanical Engineering
In Mechanics of Materials
Citations in the corpus
- A combined grain scale elastic–plastic criterion for identification of fatigue crack initiation sites in a twin containing polycrystalline nickel-base superalloy (2016, unknown): “In addition, grains oriented favorably for slip (high resolved shear stress slip systems) are observed to initiate cracks [1,14,15].”
- Sub-Grain Scale Digital Image Correlation by Electron Microscopy for Polycrystalline Materials during Elastic and Plastic Deformation (2016, background): “[1, 2] reported for the nickel-based alloy René 88DT under very high cycle fatigue loading that cracks initiated in high Schmid factor grains parallel to and slightly offset from coherent twin boundaries.”