Superelastic and cyclic response of NiTi SMA at various strain rates and temperatures
By Sia Nemat-Nasser, Weiguo Guo. 2006
317 citations recorded by the source corpus.
Subfields: Materials Chemistry
View Paper: https://www.semanticscholar.org/paper/a307ef6e245328c10ecdb114215ecdc4ff5610dc
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
Citations in the corpus
- A multi-axial, multimechanism based constitutive model for the comprehensive representation of the evolutionary response of SMAs under general thermomechanical loading conditions (2011, background): “Furthermore, significant variations in the SMA response are observed under very high rate of loading (Nemat-Nasser et al., 2005a,b; Nemat-Nasser and Guo, 2006), which cannot be explained solely on the basis of latent heat exchanges.”
- Reconciling viability and cost-effective shape memory alloy options – A review of copper and iron based shape memory metallic systems (2016, background): “It is defined as the difference between the temperatures at which 50% transformation to austenite occurs on heating and 50% transformation to martensite on cooling [19].”
- Design and Integration of a Telerobotic System for Minimally Invasive Surgery of the Throat (2009, methodology): “This strain limit was established based on our experimental evaluation and recent literature on fatigue of superelastic wires (e.g. Nemat-Nasser and Guo (2006)).”
- Effect of deformation frequency on temperature and stress oscillations in cyclic phase transition of NiTi shape memory alloy (2014, background): “…(Miyazaki et al., 1986; Tanaka et al., 1992, 1993; Strnadel et al., 1995; Abeyaratne and Kim, 1997; Ortin and Delaey, 2002; Pieczyska et al., 2005; Nemat-Nasser and Guo, 2006; Demers et al., 2009; Kang et al., 2009; Morin et al., 2011a, 2011b), the superelastic stress–strain loop drifts with the…”
- Fatigue properties of a pseudoelastic NiTi alloy: Strain ratcheting and hysteresis under cyclic tensile loading (2014, methodology): “Furthermore, NiTi tubes [17–23] were analyzed, in terms of both crack propagation rate and fatigue life estimation.”
- Welding and Joining of NiTi Shape Memory Alloys: A Review (2017, background): “For NiTi the ratio varies between 5 and 8 MPa K?”