Ceramic components manufacturing by selective laser sintering
By P. Bertrand, F. Bayle, C. Combe, P. Goeuriot, I. Smurov. 2007
337 citations recorded by the source corpus.
Subfields: Automotive Engineering, Industrial and Manufacturing Engineering, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/9e5e8c42c540f301c3064e12daceccae6540b2e1
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Automotive Engineering
- E. Herderick
- Christopher B. Williams
- Yong Chen
- Alida Mazzoli
- Yung C. Shin
- R. Hebert
- S. M. Yusuf
- N. Gao
In Industrial and Manufacturing Engineering
In Mechanical Engineering
- E. Herderick
- Christopher B. Williams
- Karthik Ramani
- H. S. C. Metselaar
- Song Zhang
- Yong Chen
- Wei Gao
- Alida Mazzoli
Citations in the corpus
- Additive manufacturing of ceramics from preceramic polymers: A versatile stereolithographic approach assisted by thiol-ene click chemistry (2019, background): “Traditional AM approaches towards ceramics rely on powder- and slurry-based technologies including stereolithography of ceramic slurries containing UV-curable photopolymers [3,4], laser sintering of ceramic powder beds [5,6] and binder jetting, where a liquid organic binder is injected into a cerami”
- Selective laser sintering in biomedical engineering (2012, background): “SLS was also investigated in the fabrication of porous structures manufactured of metals [33, 35], ceramics [2, 21, 30], and glasses [41].”
- A review on powder-based additive manufacturing for tissue engineering: selective laser sintering and inkjet 3D printing (2015, methodology): “In the powder-based method, the packing density of the powder layers is low, leading to a lower sintered density and also leading to cracks due to thermal stresses in the parts [47].”
- The status, challenges, and future of additive manufacturing in engineering (2015, positive): “The process can also be used to indirectly create ceramic [54] and metal [55] melting polymer blends; the resulting parts require high-temperature post-processing to fully sinter the structural powder.”