Environmentally Enhanced Fracture of Glass: A Historical Perspective
By S. Freiman, S. Wiederhorn, J. J. Mecholsky. 2009
166 citations recorded by the source corpus.
Subfields: Archeology, Ceramics and Composites, Earth-Surface Processes
View Paper: https://www.semanticscholar.org/paper/ff2efc232a4fe5da7caa696a96458bb28dd3abe4
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
- N. R. Silva
- P. Guess
- P. Coelho
- V. Thompson
- Y. Zhang
- E. Rekow
- Yu Zhang
Citations in the corpus
- Performance of Dental Ceramics: Challenges for Improvements (2011, background): “The mechanism responsible for this loss of strength in dental ceramics is the combined effect of stress corrosion by water molecules at the crack tip and mechanical degradation of the polycrystalline dental ceramics (Freiman et al., 2009; Salazar Marocho et al., 2010).”