Fatigue fracture of hydrogels
By Jingda Tang, Jianyu Li, J. Vlassak, Zhigang Suo. 2017
200 citations recorded by the source corpus.
Subfields: Biomedical Engineering, Molecular Medicine, Surfaces, Coatings and Films
View Paper: https://www.semanticscholar.org/paper/e83610993092267b987cc42af1d6c717fef295e4
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomedical Engineering
In Molecular Medicine
In Surfaces, Coatings and Films
Citations in the corpus
- Fatigue of double-network hydrogels (2017, methodology): “This procedure gives the thresholds of fatigue fracture as 418 J/m2 for the hydrogels prepared using the solution of 2 M AAM, 413 J/m2 for 3M AAM, and 411 J/m2 for 4 M AAM.”
- Fatigue fracture of tough hydrogels (2017, methodology): “Weuse the data of fatigue fracture in the polyacrylamide hydrogel from our previous paper [35], and plot it with the data of the tough hydrogel of the current paper.”