Visualization of water penetration in cementitious materials with superabsorbent polymers by means of neutron radiography
By Didier Snoeck, Stijn Steuperaert, K. Van Tittelboom, Peter Dubruel, N. De Belie. 2012
257 citations recorded by the source corpus.
Subfields: Civil and Structural Engineering
View Paper: https://www.semanticscholar.org/paper/e66ed442a2ffcb1dbfd675fadd145f4119cedc30
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Civil and Structural Engineering
- Didier Snoeck
- N. De Belie
- V. Mechtcherine
- C. Schröfl
- H. Wong
- N. Buenfeld
- Peter Dubruel
- K. Van Tittelboom
Citations in the corpus
- A review of characterisation methods for superabsorbent polymer (SAP) samples to be used in cement-based construction materials: report of the RILEM TC 260-RSC (2017, background): “Finally, the sorption kinetics of SAPs in cracked, cement-based, solid bodies have been explained using neutron radiography with the aim of assessing the role of SAPs in the selfsealing and self-healing of concrete [10, 39].”
- Effect of alkalinity and calcium concentration of pore solution on the swelling and ionic exchange of superabsorbent polymers in cement paste (2018, background): “These include its use as an internal curing agent to reduce self-desiccation and autogenous shrinkage in low water/cement mixtures [3-5], rheology control, frost protection [6, 7] and crack sealing/healing [8-15].”
- Effect of high amounts of superabsorbent polymers and additional water on the workability, microstructure and strength of mortars with a water-to-cement ratio of 0.50 (2014, methodology): “SAPs can be used in cementitious materials for reducing the autogenous shrinkage [3–6], for changing the rheology of the fresh material [5–7], for increasing the freeze/thaw resistance [8,9], for self-sealing [10–12] and even to promote autogenous healing [13,14].”
- Advances in characterizing and understanding the microstructure of cementitious materials (2019, background): “6(b) shows radiographic images of moisture distribution in pre-cracked mortar specimens in contact with water for 4 h [96].”
- Effect of superabsorbent polymers (SAP) on the freeze–thaw resistance of concrete: results of a RILEM interlaboratory study (2016, background): “Notable examples are: inducing an abrupt change in rheological behavior during shotcreting [6], reduction of the thermal expansion coefficient [7], reduction of fire spalling in HPC [8], and the onset of self-sealing [9] and self-healing [10].”