On the effect of deep-rolling and laser-peening on the stress-controlled low- and high-cycle fatigue behavior of Ti-6Al-4V at elevated temperatures up to 550 C
By I. Altenberger, R. Nalla, Y. Sano, L. Wagner, R. Ritchie. 2012
271 citations recorded by the source corpus.
Subfields: Ecological Modeling, Materials Chemistry, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/e3d602f18d76d4ef8f10571b97960a7c68222d39
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
- S. Rao
- G. D. Revankar
- Vinayak N. Gaitonde
- R. Shetty
Citations in the corpus
- Wear resistance enhancement of titanium alloy (Ti–6Al–4V) by ball burnishing process (2017, background): “A different microstructure is observed after deformation due to burnishing, no nanocrystallites were formed, but the dislocation arrangement consisted of diffuse tangled and debris-like structures, cell formation was not observed, and the dislocation arrangement was almost entirely planar [73].”