Overcharge-induced capacity fading analysis for large format lithium-ion batteries with LiyNi1/3Co1/3Mn1/3O2 + LiyMn2O4 composite cathode
By Minggao Ouyang, Dongsheng Ren, Languang Lu, Jianqiu Li, Xuning Feng, Xuebing Han, Guangming Liu. 2015
247 citations recorded by the source corpus.
Subfields: Automotive Engineering, Electrical and Electronic Engineering
View Paper: https://www.semanticscholar.org/paper/d83feee71e04fb998bb3c7dfd6b831347afe2515
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Automotive Engineering
In Electrical and Electronic Engineering
Citations in the corpus
- Building Safe Lithium-Ion Batteries for Electric Vehicles: A Review (2019, background): “Dendritic lithium is much easy to be formed under high charging current, overcharge, low charging temperature, improper cell balance and the uneven casting of the electrode [34].”
- A review on research status and key technologies of battery thermal management and its enhanced safety (2018, background): “Besides, thermal runaway can be induced by other unexpected abusive conditions such as mechanism crush and over discharging/charging.(87,100) Additionally, confronted the bumpiness, the battery connection accessory and its mounting structures may be twisted and deformed, thus inducing severe interna”
- Time Sequence Map for Interpreting the Thermal Runaway Mechanism of Lithium-Ion Batteries With LiNixCoyMnzO2 Cathode (2018, background): “Heating a battery can be fulfilled by oven-box heating (Dahn et al., 2013), penetration (Feng et al., 2015a; Mao et al., 2018), overcharge (Ouyang et al., 2015; Ren et al., 2017; Qi et al., 2018), power heater (Coman et al., 2017a; Gao et al., 2017), etc.”