Onset of dendritic growth in lithium/polymer cells
By M. Rosso, T. Gobron, C. Brissot, J. Chazalviel, S. Lascaud. 2001
297 citations recorded by the source corpus.
Subfields: Electrical and Electronic Engineering, Electronic, Optical and Magnetic Materials, Materials Chemistry
View Paper: https://www.semanticscholar.org/paper/d235e8788843e9673d3b5fce0ee740b61c186fba
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Electrical and Electronic Engineering
- Xuning Feng
- Minggao Ouyang
- Languang Lu
- Xuebing Han
- Q. Pang
- Xiao Liang
- L. Nazar
- Abhinandan Shyamsunder
In Electronic, Optical and Magnetic Materials
In Materials Chemistry
Citations in the corpus
- A carbon-based 3D current collector with surface protection for Li metal anode (2017, methodology): “[52, 53] to model the Li dendrite nucleation and growth process, which is expressed as follows”
- Rethinking How External Pressure Can Suppress Dendrites in Lithium Metal Batteries (2019, background): “for dendrite initiation and growth velocity in liquid electrolytes; Brownian statistical models [23-26], which analyze the morphology evolution of deposited species; and the Chazalviel electromigration-limited model [9, 27-29], which considers that dendrite initiation is induced by an electrodeposit”
- An In Vivo Formed Solid Electrolyte Surface Layer Enables Stable Plating of Li Metal (2017, methodology): “This is amplified by the non-uniform distribution of SEI that causes a high local current (J).(19,20) Utilizing an Li single-ion-conductor (ta = 0) leads to a constant cation/ion concentration (C0c/a) over the thickness of the solid electrolyte, resulting in a linear potential profile and constant e”
- A review of the internal short circuit mechanism in lithium‐ion batteries: Inducement, detection and prevention (2021, background): “At the same time, the heat is not dissipated timely, or the rate of heat generation is greater than the rate of heat dissipation, the temperature will continue to rise higher temperature at 130 C to 170 C in batteries, and there is the decomposition of separators,71 due to commercial separators for ”