Adiabatic shear banding in high speed machining of Ti-6Al-4V: experiments and modeling
By A. Molinari, C. Musquar, G. Sutter. 2002
454 citations recorded by the source corpus.
Subfields: Atomic and Molecular Physics, and Optics, Materials Chemistry, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/d23321012276778163c2b04a3b61dce9fbc537ae
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Mechanical Engineering
Citations in the corpus
- A comparative study of the cutting forces in high speed machining of Ti–6Al–4V and Inconel 718 with a round cutting edge tool (2009, unknown): “The vast majority of the published literature focuses on either Ti–6Al–4V (Su et al., 2006; Molinari et al., 2002; Baker et al., 2002; Komanduri and Hou, 2002; Barry et al., 2001; Bayoumi and Xie, 1995) or Inconel 718 (Nalbant et al.”
- Rate and thermal sensitivities of unstable transformation behavior in a shape memory alloy (2004, background): “Furthermore, self-heating is a stabilizing feature here, contrary to adiabatic shear banding instability in conventional metals (Molinari et al., 2002). Therefore, any mesh sensitivity would only be expected in the limit of isothermal behavior. Fig. 13 shows a close up of other fields across a trans”
- Finite element simulation of high-speed machining of titanium alloy (Ti–6Al–4V) based on ductile failure model (2011, background): “in 2002 [2] developed a thermo-mechanical instability model to predict the dependence of the adiabatic shear band (ASB) patterning upon the cutting velocity.”
- Modeling periodic adiabatic shear band evolution during high speed machining Ti-6Al-4V alloy (2013, methodology): “(28) to estimate the evolution degree of shear band, we have compared the predicted segment spacing with the pubulised works (Molinari et al., 2002; Cotterell and Byrne, 2008; Amin et al., 2007; Chen et al., 2011; Bäcker, 2006; Sun et al., 2009., all for Ti-6Al-4V alloy), as shown in Fig.”