Saturation of Fragmentation During Severe Plastic Deformation
By R. Pippan, S. Scheriau, A. Taylor, M. Hafok, A. Hohenwarter, A. Bachmaier. 2010
517 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/c1f077623fbfefcabe2dae6b95e74a1e17f19377
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Mechanical Engineering
Citations in the corpus
- Mechanical properties, microstructure and thermal stability of a nanocrystalline CoCrFeMnNi high-entropy alloy after severe plastic deformation (2015, background): “These methods allow deformations far beyond those possible by cold rolling and can reduce grain sizes down to the ultrafine-grained (UFG) and even nanocrystalline (NC) regimes depending on various physical and technical factors [20].”
- Design and synthesis of a magnesium alloy for room temperature hydrogen storage (2018, background): “The three intermetallic phases are well distinguished after the HPT processing for 20 and 100 turns, but their sizes become considerably smaller, as reported for many other HPT-processed multi-phase systems [20,32].”
- Thermodynamic instability of a nanocrystalline, single-phase TiZrNbHfTa alloy and its impact on the mechanical properties (2018, methodology): “For HPT processing the ideal shear strain g can be calculated using Equation (1), where r is the sample radius, t the sample thickness and n the number of rotations [33].”