Revealing electrolyte oxidation via carbonate dehydrogenation on Ni-based oxides in Li-ion batteries by in situ Fourier transform infrared spectroscopy
By Y. Zhang, Y. Katayama, R. Tatara, L. Giordano, Yang Yu, Dimitrios Fraggedakis, Jame Sun, F. Maglia, Roland Jung, Martin Z. Bazant and 1 more. Energy & Environmental Science, 2020
181 citations recorded by the source corpus.
Carbonate oxidation via dehydrogenation on LiNi0.8Co0.1Mn0.1O2 at voltages as low as 3.8 VLi was revealed by in situ FT-IR measurements.
Subfields: Automotive Engineering, Electrical and Electronic Engineering
View Paper: https://www.semanticscholar.org/paper/bc0e00c5771dd5be58970891db2faa9dd9245ca1
Citations in the corpus
- Unlocking the self-supported thermal runaway of high-energy lithium-ion batteries (2021, unknown): “Moreover, when contacting EC, the phase transformation began at 204℃, the fact that the protic species from EC dehydrogenation attacks NMC811 surface may be responsible for the reduced thermal stability 13 .”