Hydrogen-induced intergranular failure of iron
By Shuai Wang, May L. Martin, P. Sofronis, S. Ohnuki, N. Hashimoto, I. M. Robertson. 2014
254 citations recorded by the source corpus.
Subfields: Materials Chemistry, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/b59fe7fa61040cd0ce9ea26833958c0543ae50ef
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Metals and Alloys
Citations in the corpus
- Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials (2019, background): “mentioned in Section 3, recent studies of the micro structure beneath hydrogen-induced intergranular fracture surfaces [55,56] indicate th at ydrogen-enhanced plasticity and the impact”
- Hydrogen assisted crack initiation and propagation in a nickel-based superalloy (2016, background): “More importantly, they flagged up that the dislocation substructure in the hydrogen containing material is finer than in the one without hydrogen [24,27,28], which provides further support for the HELP mechanism.”
- Hydrogen embrittlement controlled by reaction of dislocation with grain boundary in alpha-iron (2018, background): “The dislocation activities around GBs will eventually yield a well-evolved dislocation structure in the volume of material just beneath the fracture surface for both the quasi-cleavage and intergranular style fracture as observed in many experiments (Martin et al., 2011a; Martin et al., 2011b; Marti”