Li7La3Zr2O12 Interface Modification for Li Dendrite Prevention.
By M. Finsterbusch, Chih‐Long Tsai, V. Roddatis, Vinod Chandra Nair, Q. Ma, S. Uhlenbruck, P. Heitjans, O. Guillon. ACS Applied Materials and Interfaces, 2016
688 citations recorded by the source corpus.
Subfields: Automotive Engineering, Electrical and Electronic Engineering
View Paper: https://www.semanticscholar.org/paper/b1e05d8d61b437619f43c6ee9ff23e9d4b2207ed
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Automotive Engineering
In Electrical and Electronic Engineering
Citations in the corpus
- Alkali Metal Anodes for Rechargeable Batteries (2019, neutral): “Owing to the difference in ionic conductivity at grain boundaries (GBs), dendrite growth along GBs where the electric field was enhanced locally during charge was found even by in situ SEM observation in some oxide-type and sulfide-based SSEs, while initial dendrite formation was mostly ascribed to ”
- Solid-State Electrolytes for Lithium-Ion Batteries: Fundamentals, Challenges and Perspectives (2019, background): “[201] proposed that the reason for this dendrite growth can be the inhomogeneous contact at the interface through carefully polishing and modifying the surface with thin Au layers.”