Atmospheric deterioration of ancient and modern hydraulic mortars
By C. Sabbioni, G. Zappia, C. Riontino, M. Blanco-Varela, J. Aguilera, F. Puertas, Koen Van Balen, E. Toumbakari. 2001
139 citations recorded by the source corpus.
Subfields: Archeology, Conservation, Earth-Surface Processes
View Paper: https://www.semanticscholar.org/paper/aebed7995dde44cb2b6a38dcc68d3f6b845b4e9a
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Archeology
In Conservation
In Earth-Surface Processes
Citations in the corpus
- MECHANICAL PROPERTIES OF NATURAL HYDRAULIC LIME-BASED MORTARS (2004, background): “The content of impurities, as silica (SiO2) and alumina (Al2O3) mainly, is the responsible for this effect [1-3].”
- Study of the mechanical behavior of masonry repair lime-based mortars cured and exposed under different conditions (2006, background): “By exposing mortar samples at different environmental conditions, different aspects of this durability were considered: outside exposure (urban atmosphere) [8], SO2 pollutant exposure [9-12], weathering cycles (in a climatic chamber) [13,14] or freezing-thawing cycles [15,16].”