Effect of tin on poly(L-lactic acid) pyrolysis
By H. Nishida, Tomokazu Mori, Shinya Hoshihara, Yujiang Fan, Y. Shirai, T. Endo. 2003
136 citations recorded by the source corpus.
Subfields: Biomaterials, Polymers and Plastics
View Paper: https://www.semanticscholar.org/paper/abcee40d3b2c5dff6059dbd42b061cee6efdd7f7
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomaterials
In Polymers and Plastics
Citations in the corpus
- Thermal degradation of poly(lactic acid) measured by thermogravimetry coupled to Fourier transform infrared spectroscopy (2009, background): “[16] also reported the effect of tin on PLLA pyrolysis.”
- Stereoblock Polylactides as High-Performance Bio-Based Polymers (2009, unknown): “107 The following SSP is first started at 140°C, and the temperature is raised up to 160°C stepwise with a 10°C increase every 10 h.”
- Thermal degradation behaviour of poly(lactic acid) stereocomplex (2004, methodology): “pyrolysis [28], the Sn content values of scPLA-ap (286 ppm) and scPLA-pr (266 ppm) samples are regarded as having nearly equal values.”