Relationships between water wettability and ice adhesion.
By Adam J. Meuler, J. David Smith, K. Varanasi, J. Mabry, G. H. McKinley, Robert E. Cohen. ACS Applied Materials and Interfaces, 2010
759 citations recorded by the source corpus.
Subfields: Aerospace Engineering, Mechanics of Materials, Surfaces, Coatings and Films
View Paper: https://www.semanticscholar.org/paper/63a756ad99e2f8d803e2525cca6bbc70e25497c9
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Aerospace Engineering
- Yongsheng Lian
- A. Work
- Nick Tepylo
- Valerie Pommier-Budinger
- Lei Jiang
- Marc Budinger
- Philseok Kim
- Jianjun Wang
In Mechanics of Materials
- Yongsheng Lian
- A. Work
- Lei Jiang
- Joanna Aizenberg
- Yanlin Song
- Nick Tepylo
- Valerie Pommier-Budinger
- Marc Budinger
In Surfaces, Coatings and Films
- Lei Jiang
- Yongsheng Lian
- A. Work
- Yanlin Song
- Joanna Aizenberg
- Tak-Sing Wong
- Jianjun Wang
- Jianyong Lv
Citations in the corpus
- Liquid-infused nanostructured surfaces with extreme anti-ice and anti-frost performance. (2012, methodology): “We have further evaluated the ice adhesion strength of SLIPS-Al and Al surfaces using a custom ice adhesion test setup based on the methods described previously (SFigure 2, movies 4 and 5).(4,15) Briefly, we formed ice in fluoroalkyl-silanized glass columns with contact areas of approximately 24 mm(”
- A novel superhydrophobic hybrid nanocomposite material prepared by surface-initiated AGET ATRP and its anti-icing properties (2014, background): “[50] Meuler A J, Smith J D, Varanasi K K, et al.”
- A survey of icephobic coatings and their potential use in a hybrid coating/active ice protection system for aerospace applications (2019, background): “The effects of hydrogen bonds on the interface bonding have been studied by many researchers [32,37,38].”
- Bio-inspired strategies for anti-icing. (2014, background): “Some researchers measured the shear strength of propelling ice off from the substrate.(33,105) The shear strength for detaching the ice layer formed between an inner cylindrical pin and an outer cylindrical mould was also used to evaluate the ice adhesion strength.”