S–N curve characteristics and subsurface crack initiation behaviour in ultra‐long life fatigue of a high carbon‐chromium bearing steel
By K. Shiozawa, L. Lu, S. Ishihara. 2001
339 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanics of Materials
View Paper: https://www.semanticscholar.org/paper/9b7a6956b8fd394c25f965006654db4597f03183
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Mechanics of Materials
Citations in the corpus
- Propensities of crack interior initiation and early growth for very-high-cycle fatigue of high strength steels (2014, methodology): “For the material tested in this investigation, we noticed a similar case for the crack growth data [10] and obtained the values of A = 1.”
- The formation mechanism of characteristic region at crack initiation for very-high-cycle fatigue of high-strength steels (2016, background): “FGA is also called optical dark area (ODA) [11] or granular bright facet (GBF) [16].”