Temperature dependent, large electromechanical strain in Nd-doped BiFeO3-BaTiO3 lead-free ceramics
By Dawei Wang, Amir Khesro, S. Murakami, A. Feteira, Quanliang Zhao, I. Reaney. 2017
204 citations recorded by the source corpus.
Lead-free piezoceramics with the composition 0.7(Bi1-xNdx)FeO3-0.3BaTiO3+0.1 wt% MnO2 (BNxF-BT) were prepared using a conventional solid state route. X-ray diffraction and temperature dependent permittivity measurements indicated a transition from a composition lying at a morphotropic phase boundary (MPB) to a pseudocubic phase as a function of Nd concentration. The highest maximum strain (Smax ∼ 0.2% at 60 kV/cm) and effective piezoelectric coefficient (d33* = 333 pm/V) were obtained at room temperature for the composition BN0.02F-BT. The decrease in remanent polarization (Pr) and Berlincourt d33 with increase in Nd concentration can be attributed to the coexistence of ferroelectric and relaxor phases. In-situ polarisation and strain measurements revealed an increase in Pr and d33* with temperature and a reduction in the coercive field EC. Presumably this behavior is due to a combination of thermally activated domain wall motion and lowering of the activation energy for a field induced relaxor-ferroelectric transition, as the Curie maximum is approached.
Subfields: Electronic, Optical and Magnetic Materials, Materials Chemistry
View Paper: https://www.semanticscholar.org/paper/9b64720bcfb7142c60dec5d8c54c8f32fcf05bea
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Electronic, Optical and Magnetic Materials
In Materials Chemistry
Citations in the corpus