Melt Pool Characterization for Selective Laser Melting of Ti-6Al-4V Pre-Alloyed Powder
By Hai-jun Gong, H. Gu, K. Zeng, J. Dilip, D. Pal, B. Stucker, D. Christiansen, J. Lewandowski. 2014
159 citations recorded by the source corpus.
View Paper: https://www.semanticscholar.org/paper/97f643490dcaa67477ef00e800f19a970c4dd701
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
- T. DebRoy
- T. Mukherjee
- N. Lavery
- J. A. Cherry
- S. Mehmood
- B. Girling
- H. Davies
- E. Sackett
Citations in the corpus
- Mitigation of lack of fusion defects in powder bed fusion additive manufacturing (2018, background): “Slower scanning speed was also found to reduce lack of fusion defect for titanium alloys [4,6,7,12,13] and aluminum alloys [8–10].”
- Effects of hot isostatic pressing on the elastic modulus and tensile properties of 316L parts made by powder bed laser fusion (2017, background): “15 welding and more recently in powder bed laser fusion [46], [56], [57]– when temperatures in the melt-pool rise above the vaporisation temperature of the various alloy components and a plasma is formed, enhancing laser absorption.”