Cementite decomposition in heavily drawn pearlite steel wire
By K. Hono, M. Ohnuma, M. Murayama, S. Nishida, A. Yoshie, T. Takahashi. 2001
243 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanical Engineering, Mechanics of Materials
View Paper: https://www.semanticscholar.org/paper/938e2121c7ef7cafdec403a052d1256094627bdc
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Mechanical Engineering
In Mechanics of Materials
Citations in the corpus
- White structure flaking (WSF) in wind turbine gearbox bearings: Effects of ‘butterflies’ and white etching cracks (WECs) (2012, background): “Since carbon has poor solubility in ferrite, carbon must be accommodated by lattice defects such as vacancies, vacancy–carbon complexes, dislocation cores forming Cottrell atmosphere and the large grain boundary area.(26,47,114) Dislocation density of WEA in butterfly wings is estimated as about 10(”
- Grain boundary segregation engineering in metallic alloys: A pathway to the design of interfaces (2014, unknown): “cells [67,68], superconductors [69], or ceramics [60–66] we focus here on recent developments pertaining to metallic alloys used for structural applications [70–82].”