Wear of nano-structured carbide-free bainitic steels under dry rolling–sliding conditions
By A. Leiro, E. Vuorinen, K. Sundin, B. Prakash, T. Sourmail, V. Smanio, F. G. Caballero, C. García-Mateo, R. Elvira. 2013
174 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/8f16b4a72ffec30280338801b9c0db493a9588f8
Citations in the corpus
- Three-body abrasive wear of fine pearlite, nanostructured bainite and martensite (2013, unknown): “The dry rolling-sliding wear of series of steels said to contain carbide-free bainite has been reported recently [6] (a high slip of ∼ 5% was used in the test programme); here, the carbide-free bainitic steels were shown to exhibit significantly lower rates of wear (∼ 50%) than a steel with a lower ”