Effect of nano-TiB2 particles on the anisotropy in an AlSi10Mg alloy processed by selective laser melting
By Yinglin Xiao, Z. Bian, Y. Wu, G. Ji, Y. Q. Li, Michael Li, Q. Lian, Zhe Chen, Ahmed Addad, Wang Huiya. Journal of Alloys and Compounds, 2019
162 citations recorded by the source corpus.
Abstract In components built by selective laser melting (SLM), possible anisotropy in microstructure significantly affects mechanical properties (i.e. service performance) and there is a constant effort to solve this problem. This work carried out a comparative study using fully dense AlSi10Mg alloy and in-situ nano-TiB2 decorated AlSi10Mg composite samples processed by SLM. The aim was at clarifying the effect of integrated nanoparticles on the anisotropy of the as-built component. Microstructure and texture evolution were investigated by scanning and transmission electron microscopy, electron backscatter diffraction, X-ray and neutron diffraction. The SLMed AlSi10Mg sample shows a coarse columnar grain structure with and fiber orientation texture and obvious anisotropy in mechanical properties. However, the nano-TiB2 modified AlSi10Mg sample exhibits fine equiaxed grains, no preferred crystallographic texture and remarkably reduced anisotropy. Besides, both tensile strength and ductility have been improved in the SLMed TiB2 decorated AlSi10Mg sample. The preliminary mechanism upon grain refinement effect due to nano-TiB2 particles on columnar-to-equiaxed transition and reduction of anisotropy was discussed.
Subfields: Automotive Engineering, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/7ec5907bc3d27d649e5fba401251d6983770d3c1
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Mechanical Engineering
Citations in the corpus
- A review of Laser Powder Bed Fusion Additive Manufacturing of aluminium alloys: Microstructure and properties (2021, methodology): “The grain sizes were refined to 20–35 μm, and the mechanical properties of the components were enhanced, in contrast to columnar structures with length of 60 μm to 1.6 mm without the addition of TiB2.”