Last-stage solidification of alloys: Theoretical model of dendrite-arm and grain coalescence
By M. Rappaz, A. Jacot, W. Boettinger. 2003
294 citations recorded by the source corpus.
AbstractHot tearing in castings is closely related to the difficulty of bridging or coalescence of dendrite arms during the last stage of solidification. The details of the process determine the temperature at which a coherent solid forms; i.e., a solid that can sustain tensile stresses. Based on the disjoining-pressure concept used in fluid dynamics, a theoretical framework is established for the coalescence of primary-phase dendritic arms within a single grain or at grain boundaries. For pure substances, approaching planar liquid/solid interfaces coalesce to a grain boundary at an undercooling (ΔTb), given by $$\Delta T_b = \frac{{\Delta \Gamma _b }}{\delta } = \frac{{\gamma _{gb} - 2\gamma _{sl} }}{{\Delta s_f }}\frac{1}{\delta }$$ where δ is the thickness of an isolated solid-liquid interface, and ΔГb is the difference between the grain-boundary energy, γgb, and twice the solid/liquid interfacial energy, 2γsl, divided by the entropy of fusion. If γgb<2γsl, then ΔTb<0 and the liquid film is unstable. Coalescence occurs as soon as the two interfaces get close enough (at a distance on the order of δ). This situation, typical of dendrite arms belonging to the same grain (i.e., γgb=0), is referred to as “attractive”. The situation where γgb=2 γsl is referred to as “neutral”; i.e., coalescence occurs at zero undercooling. If γgb>2γsl, the two liquid/solid interfaces are “repulsive” and ΔTb>0. In this case, a stable liquid film between adjacent dendrite arms located across such grain boundaries can remain until the undercooling exceeds ΔTb. For alloys, coalescence is also influenced by the concentration of the liquid film. The temperature and concentration of the liquid film must reach a coalescence line parallel to, but ΔTb below, the liquidus line before coalescence can occur. Using one-dimensional (1-D) interface tracking calculations, diffusion in the solid phase perpendicular to the interface (backdiffusion) is shown to aid the coalescence process. To study the interaction of interface curvature and diffusion in the liquid film parallel to the interface, a multiphase-field approach has been used. After validating the method with the 1-D interface tracking results for pure substances and alloys, it is then applied to two-dimensional (2-D) situations for binary alloys. The coalescence process is shown to originate in small necks and involve rapidly changing liquid/solid interface curvatures.
Subfields: Aerospace Engineering, Materials Chemistry, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/79856ed1a89c9c389a47e8cc154f371e6c10e93a
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Aerospace Engineering
In Materials Chemistry
In Mechanical Engineering
Citations in the corpus
- Hot cracking mechanism affecting a non-weldable Ni-based superalloy produced by selective electron Beam Melting (2018, background): “[34], Rappaz relied on the concept of “attractive” and “repulsive” boundaries depending on the crystallographic misorientation.”
- Progress in modelling solidification microstructures in metals and alloys. Part II: dendrites from 2001 to 2018 (2020, methodology): “The results correspond to Rappaz et al. ’ s theory of coalescence of two solid – liquid interfaces [67].”