On the role of axial load and the effect of interface position on the tensile strength of a friction stir welded aluminium alloy
By K. Sharvan Kumar, S. Kailas. 2008
155 citations recorded by the source corpus.
Subfields: Aerospace Engineering, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/735d88555a004abaff7e9396c0430da06503fb23
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Aerospace Engineering
In Mechanical Engineering
Citations in the corpus
- Investigations on the effects of friction stir welding parameters on intermetallic and defect formation in joining aluminum alloy to mild steel (2013, background): “Kumar and Kailas [29] reported that the increase in the plunge depth of the tool by 0.8 mm increased the axial load from 4 to 104 kN.”
- Tensile properties of friction stir welded joints of 2024 aluminum alloys in different heat-treated-state (2009, background): “Many studies have focused on the mechanical properties of FSW joints of heat-treatable aluminum alloys such as 2017T351 [13], 2195-T8 [15], 7020-T6 [16], 6061 [3,17], 6063 [8,10] and 6082 [18].”