Degradation observations of encapsulated planar CH3NH3PbI3 perovskite solar cells at high temperatures and humidity
By Yuanyuan Han, Steffen Meyer, Yasmina Dkhissi, Karl Weber, J. Pringle, U. Bach, L. Spiccia, Yi-bing Cheng. 2015
765 citations recorded by the source corpus.
Subfields: Electrical and Electronic Engineering, Materials Chemistry
View Paper: https://www.semanticscholar.org/paper/723a9f9631f15cee0c085aa4d1492cd200ff4af4
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Electrical and Electronic Engineering
- Martin A. Green
- Ewan D. Dunlop
- Yoshihiro Hishikawa
- Wilhelm Warta
- K. Emery
- A. Ho-baillie
- D. Levi
- H. Snaith
In Materials Chemistry
- Martin A. Green
- A. Ho-baillie
- Md. K. Nazeeruddin
- Ewan D. Dunlop
- G. Grancini
- Yoshihiro Hishikawa
- Wilhelm Warta
- K. Emery
Citations in the corpus
- Solar cell efficiency tables (version 57) (2020, background): “Han et al.(21) and Yang and You(22) review the stability of similar devices.”
- Encapsulation of Organic and Perovskite Solar Cells: A Review (2019, background): “However, the device performance quickly decreased to <50% of the initial efficiency within 10 h under constant illumination and at an ambient humidity of 80% and cell temperature of 85 ◦C [65].”
- Solar cell efficiency tables (Version 55) (2019, methodology): “emerging technologies, Pb‐halide perovskite cells may not demonstrate the same level of stability as conventional cells, with the stability of such perovskite cells discussed elsewhere.(7,8) For the present device, the assigned efficiency was based on a “settled power at fixed voltage” (SPFV) measur”