Mechanical properties of porous titanium compacts prepared by powder sintering
By Ik-Hyun Oh, N. Nomura, N. Masahashi, S. Hanada. 2003
569 citations recorded by the source corpus.
Subfields: Biomedical Engineering, Materials Chemistry, Surgery
View Paper: https://www.semanticscholar.org/paper/70bd3f913f89ea410bc79f0d12511e4b8ea8e8d9
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Surgery
Citations in the corpus
- Fabrication methods of porous metals for use in orthopaedic applications. (2006, methodology): “sintered spherical unalloyed titanium powders with and without applied pressure and achieved a porosity range of 5–37% [62].”
- Ti-6Al-4V triply periodic minimal surface structures for bone implants fabricated via selective laser melting. (2015, background): “Nowadays, conventional techniques available for the fabrication of open-cell porous titanium structures mainly include controlled powder sintering (Oh et al., 2003), polymeric sponge relication (Li et al., 2005), molding and sintering of short metal fibres (Galante et al., 1973) and solid-state…”
- New Developments of Ti-Based Alloys for Biomedical Applications (2014, methodology): “For loose sintered powders, the pore size, volume fraction, shape and distribution throughout the sample thickness and the inter particle neck size have a major impact on the mechanical properties of the resulting material [51].”