Microstructural evolution in adiabatic shear bands in Ta and Ta–W alloys
By M. Pérez‐Prado, J. A. Hines, Kenneth S. Vecchio. 2001
196 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanics of Materials
View Paper: https://www.semanticscholar.org/paper/6ff9d1605ec47da7573beda112e6a971b413158d
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Mechanics of Materials
Citations in the corpus
- Thermo-Mechanical Aspects of Adiabatic Shear Failure of AM50 and Ti6Al4V Alloys (2008, background): “DRX will definitely cause local softening of the material, while being driven by mechanical strain rather than temperature (Hines and Vecchio, 1997; Perez-Prado et al., 2001).”
- Mechanical behavior and microstructure of Ti20Hf20Zr20Ta20Nb20 high-entropy alloy loaded under quasi-static and dynamic compression conditions (2016, background): “Nevertheless, in the case of Ta and Ta-W alloys it was reported [66] that grain refinement by DRX is a sluggish process that cannot take place in a short period of time such as the duration of the present impact test (~10−4 s).”