Very Low Conductivity Threshold in Bulk Isotropic Single‐Walled Carbon Nanotube–Epoxy Composites
By M. Bryning, M. F. Islam, J. Kikkawa, Arjun G. Yodh. 2005
596 citations recorded by the source corpus.
Subfields: Materials Chemistry, Polymers and Plastics
View Paper: https://www.semanticscholar.org/paper/5de11e134b730543db4b7673571ae6cb46bc2551
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Polymers and Plastics
Citations in the corpus
- Multiscale hybrid micro-nanocomposites based on carbon nanotubes and carbon fibers (2010, unknown): “The low loadings of CNTs often employed in epoxy resins imply less inhomogenities but also less positive perturbations of mechanical properties [53].”
- NANOTUBES AS POLYMERS (2009, unknown): “005 vol% to 11 vol% [244,245].”
- Dispersion of Carbon Nanotubes: Mixing, Sonication, Stabilization, and Composite Properties (2012, background): “It had been demonstrated that a partially re-aggregated state (after long time mixing) shows a lower percolation threshold than the original well-mixed state [60,61].”
- Self-heating fiber reinforced polymer composite using meso/macropore carbon nanotube paper and its application in deicing (2014, unknown): “[32] Bryning MB, Islam MF, Kikkawa JM, Yodh AG.”
- The influence of single-walled carbon nanotube structure on the electromagnetic interference shielding efficiency of its epoxy composites (2007, methodology): “016 the conductivity and percolation behavior of composites [21].”
- Fundamentals, processes and applications of high-permittivity polymer–matrix composites (2012, background): “Rope formation is energetically favorable due to the Van der Waals attractions or other interactions between isolated nanotubes [226].”
- Reflection and absorption contributions to the electromagnetic interference shielding of single-walled carbon nanotube/polyurethane composites (2007, methodology): “These included SWCNT composites with critical exponent values of 1.5 for polyimide [30], 1.3 and 2.68 for epoxy [10,28], and 2–3 for different SWCNT materials with epoxy [ 8 ].”