Modification of poly(lactic acid) films: Enhanced wettability from surface-confined photografting and increased degradation rate due to an artifact of the photografting process
By A. Janorkar, A. Metters, D. Hirt. 2004
167 citations recorded by the source corpus.
Subfields: Biomaterials, Biomedical Engineering, Surfaces, Coatings and Films
View Paper: https://www.semanticscholar.org/paper/5d7d469668eeff3118fdb2c666630b4385f99b9d
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomaterials
In Biomedical Engineering
In Surfaces, Coatings and Films
Citations in the corpus
- Review: Photopolymerizable and Degradable Biomaterials for Tissue Engineering Applications (2007, unknown): “with PAA and poly(acrylamide) using photopolymerization in an attempt to generate a bioactive surface with rapid degradation.(99) Various copolymers containing blocks of poly(a-hydroxy esters) and other synthetic polymers have been prepared.”
- Surface Modification of 3D Printed PLA Objects by Fused Deposition Modeling: A Review (2019, background): “As a result, it has been observed that the hydrophilicity or wettability of the grafted surfaces has improved considerably [86].”
- Hydrolysis and Biodegradation of Poly(lactic acid) (2017, background): “• generation of hydrophilic surfaces by copolymerization, grafting reactions, and cross-linking [84-90]”