Response of Ti–6Al–4V and Ti–24Al–11Nb alloys to dry sliding wear against hardened steel
By Md.Ohidul Alam, Abdul Haseeb. 2002
171 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanics of Materials
View Paper: https://www.semanticscholar.org/paper/556c88ea1bdccf287e96b430088c6eaac313b1be
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
- X. X. Li
- S. Rao
- G. D. Revankar
- Vinayak N. Gaitonde
- R. Shetty
- X. Ji
- Ya-zhen Li
- Zhou Yuepeng
Citations in the corpus
- Wear resistance enhancement of titanium alloy (Ti–6Al–4V) by ball burnishing process (2017, background): “Alam Ohidul and Haseeb [9] investigated the tribological properties of Ti–6Al–4V and Ti–24Al–11Nb alloys subjected to dry sliding wear against hardened-steel and found that the lower wear rate of Ti–6Al–4Valloy alloy was linked to severe delamination wear.”
- Effects of sliding velocity on tribo-oxides and wear behavior of Ti–6Al–4V alloy (2015, background): “It is well known that titanium alloys possess notoriously poor sliding wear resistance [1–11].”