Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V
By C. Qiu, N. Adkins, Moataz M. Attallah. 2013
755 citations recorded by the source corpus.
Subfields: Automotive Engineering, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/4ff94c7a52ee10ab38066efa6b4d8b28efa1632e
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Automotive Engineering
In Mechanical Engineering
Citations in the corpus
- Effects of hot isostatic pressing on the elastic modulus and tensile properties of 316L parts made by powder bed laser fusion (2017, background): “The effects on mechanical properties of surface finishing, heat treatments and hot isostatic pressing are then examined, and for Ti-6Al-4V this is done for powder bed [7], [12] and for electron beam [11].”
- An experimental study of residual stress and direction-dependence of fatigue crack growth behaviour in as-built and stress-relieved selective-laser-melted Ti6Al4V (2019, background): “[21,24,26,29,30] of parts produced by SLM processing.”
- Fatigue of additive manufactured Ti-6Al-4V, Part II: The relationship between microstructure, material cyclic properties, and component performance (2020, background): “For non-heat treated and annealed conditions in the literature, for example in [10,51,66,67], build orientation anisotropy of fatigue performance has been reported.”