Ferromagnetism as a universal feature of nanoparticles of the otherwise nonmagnetic oxides
By A. Sundaresan, R. Bhargavi, N. Rangarajan, U. Siddesh, C. Rao. 2006
1,247 citations recorded by the source corpus.
Room-temperature ferromagnetism has been observed in nanoparticles $(7\char21{}30\phantom{\rule{0.3em}{0ex}}\mathrm{nm}\phantom{\rule{0.2em}{0ex}}\mathrm{diam})$ of nonmagnetic oxides such as ${\mathrm{CeO}}_{2}$, ${\mathrm{Al}}_{2}{\mathrm{O}}_{3}$, $\mathrm{ZnO}$, ${\mathrm{In}}_{2}{\mathrm{O}}_{3}$, and ${\mathrm{SnO}}_{2}$. The saturated magnetic moments in ${\mathrm{CeO}}_{2}$ and ${\mathrm{Al}}_{2}{\mathrm{O}}_{3}$ nanoparticles are comparable to those observed in transition-metal-doped wideband semiconducting oxides. The other oxide nanoparticles show somewhat lower values of magnetization but with a clear hysteretic behavior. Conversely, the bulk samples obtained by sintering the nanoparticles at high temperatures in air or oxygen became diamagnetic. As there were no magnetic impurities present, we assume that the origin of ferromagnetism may be the exchange interactions between localized electron spin moments resulting from oxygen vacancies at the surfaces of nanoparticles. We suggest that ferromagnetism may be a universal characteristic of nanoparticles of metal oxides.
Subfields: Electronic, Optical and Magnetic Materials, Materials Chemistry
View Paper: https://www.semanticscholar.org/paper/482eb0d961d7103f83e1a5b11dd4ef7fc7fd7ca1
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
- V. Markovich
- G. Jung
- R. Puźniak
- A. Wisniewski
- A. Kohn
- Kiyonori Suzuki
- Xiaodong Wu
- O. V. Belousova
Citations in the corpus
- Structural, optical, XPS and magnetic properties of Zn particles capped by ZnO nanoparticles (2015, result): “27 emu/g (Z17), which was found to be a higher value in comparison to the literature one (from 6 10 to 6 10 emu/g) for non-doped ZnO nanoparticles of various sizes in the range of 4–500 nm [19,22,26,39,45,73–75].”