Internal and surface damage of multiphase steels and pure iron after electrochemical hydrogen charging
By D. P. Escobar, C. Miñambres, L. Duprez, K. Verbeken, M. Verhaege. 2011
197 citations recorded by the source corpus.
Subfields: Civil and Structural Engineering, Materials Chemistry, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/3ec25a51ba1ff75c5c7d9f69922e15ccbf1cd0d2
Citations in the corpus
- Effect of microstructure and composition on hydrogen permeation in X70 pipeline steels (2013, unknown): “[48] have demonstrated by etching with LePera reagent that Mn segregation occurs in hot rolled steels.”
- Determination of the hydrogen fugacity during electrolytic charging of steel (2014, unknown): “These conditions depend on (i) the chemical composition of the steel, (ii) its microstructure, (iii) the electrolyte and (iv) the sample preparation [65, 66].”