Low-fired fluoride microwave dielectric ceramics with low dielectric loss
By Xiaoqiang Song, K. Du, Jie Li, Xuekai Lan, Wen‐Zhong Lu, Xiaohong Wang, W. Lei. Ceramics International, 2019
162 citations recorded by the source corpus.
Abstract Low-fired fluoride microwave dielectric ceramics (LiF, CaF2, SrF2 and BaF2) were prepared through a simple one-step sintering process. Fluoride ceramics, especially LiF, which had the lowest sintering temperature of 800 °C, could be well sintered below 1050 °C. Rietveld refinement results showed that LiF, CaF2, SrF2 and BaF2 ceramics crystallized into a cubic structure with space group Fm-3m. The relative permittivity (er), quality factor (Q × f) and temperature coefficient of the resonant frequency (τf) of the fluoride ceramics were closely related to relative density, the ionic polarizability of the primitive unit cell, the packing fraction and the bond valence. In this series of low-permittivity fluoride ceramics, LiF, CaF2 and BaF2 could be co-fired with Ag powders, and LiF ceramic exhibited the highest Q×f value of 73880 GHz, which is comparable to those of traditional oxide microwave dielectric ceramics.
Subfields: Electrical and Electronic Engineering, Electronic, Optical and Magnetic Materials, Materials Chemistry
View Paper: https://www.semanticscholar.org/paper/361c1a104cc47a518e7d8f2aed93ef750f82b158