Evaluation of a novel approach to a delamination factor after drilling composite laminates using a core–saw drill
By Chung-Chen Tsao, K. Kuo, I. Hsu. 2012
141 citations recorded by the source corpus.
Subfields: Biomedical Engineering, Electrical and Electronic Engineering, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/3498c9b3577580e5aad4649ef41dda07a2349381
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomedical Engineering
In Electrical and Electronic Engineering
In Mechanical Engineering
Citations in the corpus
- Assessment of delamination in composite materials: A review (2016, methodology): “Ad A Mohan et al., 15 Krishnaraj et al.35 and Pinho et al.36 5 Damage ratio DRAT = DMAR AAVG Mehta et al.14 and Sereshk and Bidhendi20 6 Adjusted delamination factor (Fda) Fda = Fd + Ad F 2 d Fdð Þ Amax AO Davim et al., 16 Campos Rubio et.al.,26 Karimi et al.37 and Sereshk and Bidhendi20 7 Equivalen”
- Cryogenic cooling-induced process performance and surface integrity in drilling CFRP composite material (2016, background): “In the literature, various cutting speeds [6], feed rate [3, 7], drill bit geometries [8–11], tool coatings [12, 13], and tool materials [14, 7] have been proposed to minimize delamination in drilling of CFRP composite materials.”