Hydrogen thermal desorption relevant to delayed-fracture susceptibility of high-strength steels
By M. Nagumo, M. Nakamura, Kenichi Takai. 2001
302 citations recorded by the source corpus.
Subfields: Materials Chemistry, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/29ee379ab6a73d8358ffd35bfd5368fe5d4797a8
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Metals and Alloys
- Dierk Raabe
- K. Tsuzaki
- Motomichi Koyama
- E. Akiyama
- C. Tasan
- Kenichi Takai
- Rajagopalan Srinivasan
- T. Neeraj
Citations in the corpus
- The Interaction of Dislocations and Hydrogen-vacancy Complexes and Its Importance for Deformation- induced Proto Nano-voids Formation in α-Fe (2015, background): “It was proposed that plasticity-generated, hydrogen stabilized vacancy damage and vacancy aggregation were the primary cause for nano-voiding (Neeraj et al., 2012).”
- Recent progress in microstructural hydrogen mapping in steels: Quantification, kinetic analysis, and multi-scale characterisation (2017, background): “The latter dependence is known as hydrogen-induced delayed fracture [53,54,56].”