Effects of fly ash characteristics and alkaline activator components on compressive strength of fly ash-based geopolymer mortar
By M. Hadi, Mustafa Al-Azzawi, Tao Yu. Construction and Building Materials, 2018
172 citations recorded by the source corpus.
Abstract The compressive strength of fly ash-based geopolymer mortar (FBGM) made from five different sources of fly ash was examined. The weight ratio of alkaline activator to fly ash content (AL/FA), the weight ratio of sodium silicate to sodium hydroxide (Na2SiO3/NaOH) and concentration of the NaOH were considered the main parameters. A total of 180 FBGM mixes were prepared and tested for compressive strength. The results indicated that the optimum AL/FA ratio for activating fly ashes was in the range of 0.5 and 0.6. The compressive strength of the FBGM that were mixed with different fly ashes exhibited different response to the increase of the Na2SiO3/NaOH ratio and NaOH concentration. Fly ashes with a high content of fine particles and amorphous components such as SiO2 and Al2O3 activated at a low dosage of Na2SiO3/NaOH ratio and NaOH. While the activation of fly ashes with a low content of fine particles and amorphous components required a high dosage of Na2SiO3/NaOH ratio and NaOH. An artificial neural network was developed and the analytical results showed high performance in predicting the compressive strengths of the FBGM.
Subfields: Civil and Structural Engineering, Materials Chemistry
View Paper: https://www.semanticscholar.org/paper/24a1fd3b376fed488617be57efd7a0069a3be224
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Civil and Structural Engineering
In Materials Chemistry
Citations in the corpus
- The Durability of Alkali-Activated Materials in Comparison with Ordinary Portland Cements and Concretes: A Review (2020, background): “There is no standard, and just a few recommendations have been made; for example, FA-based AAM needs a high concentration of NaOH solution, and curing at 60 C for 48 h will result in more complete polymerization [114,115].”