Mechanical and thermal properties of sisal fiber-reinforced rubber seed oil-based polyurethane composites
By I. O. Bakare, F. Okieimen, C. Pavithran, H. P. S. Abdul Khalil, M. Brahmakumar. 2010
188 citations recorded by the source corpus.
Subfields: Polymers and Plastics
View Paper: https://www.semanticscholar.org/paper/22964427cababa74bf5d696b59c919d85dd20c1a
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Polymers and Plastics
- T. Sathishkumar
- M. Gupta
- P. Sahu
- N. Rajini
- Subramaniam Shankar
- R. Rajasekar
- P. Navaneethakrishnan
- S. Saravanakumar
Citations in the corpus
- Targeted pre-treatment of hemp bast fibres for optimal performance in biocomposite materials: A review (2017, unknown): “…90 − 120 1.5 9 75 (Pekala et al. 1992; Voigt et al. 2003) (Hagstrand and Oksman 2001) Polyurethane 80 − 125 1.2 0.43 4.8 (Rozman et al. 2003; SaintMichel et al. 2006; Bakare et al. 2010) (Hufenbach et al. 2013) Furan 40 − 90 1.3 3 − 8.5 30 − 60 (Eisenreich 2008; Džalto et al. 2014;…”
- Vegetal fibers in polymeric composites: a review (2015, background): “Polyurethane (PU) banana [148], coconut [149], curaua [108], sisal [150,151]”
- Water absorption behavior of cellulosic fibres polymer composites: A review on its effects and remedies (2020, methodology): “[89] fabricated the composites utilizing sisal fibre and rubber seed oil-based polyurethane to interpret the consequences of 30 days water immersion on their mechanical properties.”
- Characterization of natural fiber and composites – A review (2013, background): “Yi et al.34 concluded that during TGA, the sisal fiber lignin content was degraded in the temperature range from 60 to 200 C and up to 350 C, and most of the cellulose was decomposed by thermal depolymerization of hemicellulose and the cleavage of the glycosidic linkage of cellulose at 350 C. Simila”