Hydrogen environment embrittlement of stable austenitic steels
By T. Michler, C. S. Marchi, J. Naumann, S. Weber, Mauro Martin. 2012
197 citations recorded by the source corpus.
Subfields: Mechanical Engineering, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/1baf0cf953dec755db7b8964c0b962f5eec834c5
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Mechanical Engineering
- Dierk Raabe
- O. A. Zambrano
- Motomichi Koyama
- K. Tsuzaki
- E. Akiyama
- Young‐kook Lee
- H. Springer
- P. Sofronis
In Metals and Alloys
Citations in the corpus
- Hydrogen embrittlement associated with strain localization in a precipitation-hardened Fe–Mn–Al–C light weight austenitic steel (2014, background): “However, as hydrogen embrittlement occurs preferably in strain-localized regions, this sliplocalization trend observed in TRIPLEX steels is speculated to have an influence on hydrogen embrittlement, which is of high importance for using in hydrogen-related infrastructures such as a hydrogen storage ”
- Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials (2019, background): “While which deformation mode is dominant will evidently affect the austenitic steel’s performance in a hydrogen environment, it was found that hydrogen susceptibility is not correlated with SFE [101], suggesting that hydrogen embrittlement is not necessarily dependent on the deformation mode.”
- Determination of the hydrogen fugacity during electrolytic charging of steel (2014, unknown): “1 Importance Hydrogen has caused catastrophic failures in service, and there are many studies into the influence of hydrogen on the mechanical properties of steels [1-64].”
- Overview of hydrogen embrittlement in high-Mn steels (2017, background): “16 e Hydrogen embrittlement susceptibility of high-Mn steels in a 10 MPa high-pressure hydrogen gas atmosphere [30,118].”