Polyethylene characterization by FTIR
By J. V. Gulmine, P. R. Janissek, H. Heise, L. Akcelrud. 2002
759 citations recorded by the source corpus.
Subfields: Analytical Chemistry, Polymers and Plastics
View Paper: https://www.semanticscholar.org/paper/15275c7301b4b5e2a96d251604bbffaa68f8ad83
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
Citations in the corpus
- Enhanced Visible Light Photodegradation of Microplastic Fragments with Plasmonic Platinum/Zinc Oxide Nanorod Photocatalysts (2019, background): “Compared to un-irradiated LDPE fragments, several functional groups can be identified having peaks at 710 cm-1, and 719 cm-1 (medium type rocking deformation of -CH2), 2847 cm-1, 2915 cm-1 (symmetric and asymmetric strong stretching of -CH2), 1462 cm-1, 1472 cm-1 (stretching of -C=C- bond), and 1377”