Determination of the critical hydrogen concentration for delayed fracture of high strength steel by constant load test and numerical calculation
By Maoqiu Wang, E. Akiyama, K. Tsuzaki. 2006
144 citations recorded by the source corpus.
Subfields: Materials Chemistry, Mechanical Engineering, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/13d2f6d47f9dd4d5bb016df7b2e5e36026f3facb
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
- Dierk Raabe
- K. Tsuzaki
- Motomichi Koyama
- E. Akiyama
- C. Tasan
- O. A. Zambrano
- Kenichi Takai
- M. Rohwerder
In Mechanical Engineering
In Metals and Alloys
- Dierk Raabe
- K. Tsuzaki
- Motomichi Koyama
- E. Akiyama
- C. Tasan
- Kenichi Takai
- O. A. Zambrano
- Young‐kook Lee
Citations in the corpus
- Recent progress in microstructural hydrogen mapping in steels: Quantification, kinetic analysis, and multi-scale characterisation (2017, background): “The latter dependence is known as hydrogen-induced delayed fracture [53,54,56].”