Spectroscopic identification of protective and non-protective corrosion coatings on steel structures in marine environments
By D. Cook. 2005
165 citations recorded by the source corpus.
Subfields: Environmental Chemistry, Materials Chemistry, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/0d230f20ade3d959b1e6c90999fcebd011badde2
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Environmental Chemistry
In Materials Chemistry
In Metals and Alloys
Citations in the corpus
- Weathering steels: From empirical development to scientific design. A review (2014, methodology): “In 1999 Cook et al. [122], using a wide range of high resolution spectroscopic instrumentation (XRD, IR, MS, micro Raman, EPMA, EDX, and SEM), analysed the mass fraction of each oxide present in ASTM A-588 WS [123] exposed in a rural atmosphere for 16 years.”
- Long-term atmospheric corrosion of mild steel (2011, background): “Other phases usually present in the steel corrosion products are magnetite (Fe 3 O 4 ) or maghemite ( γ -Fe 2 O 3 ), which cannot be differentiated by XRD due to their similar crystalline structure [24].”
- On the penetration of corrosion products from reinforcing steel into concrete due to chloride-induced corrosion (2010, background): “These are the expected iron oxides that form at high temperatures [31].”