Pyrolysis of mixed plastics for the recovery of useful products
By M. Siddiqui, H. Redhwi. 2009
190 citations recorded by the source corpus.
Subfields: Biomedical Engineering, Industrial and Manufacturing Engineering, Polymers and Plastics
View Paper: https://www.semanticscholar.org/paper/0c996ba4f9cdbc5528c70d21616c14868763798c
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomedical Engineering
In Industrial and Manufacturing Engineering
In Polymers and Plastics
Citations in the corpus
- Valorization of packaging plastic waste by slow pyrolysis (2018, background): “…of plastics is generally carried out at fast heating rate to a final temperature up to 700 °C or at moderate temperature (∼500 °C) in presence of catalyst (Chattopadhyay et al., 2016; Kaminsky et al., 1995; Kumar et al., 2011; Siddiqui and Redhwi, 2009; Williams and Williams, 1997a, 1999b).”
- Pyrolysis gases produced from individual and mixed PE, PP, PS, PVC, and PET—Part I: Production and physical properties (2018, background): “Examples include the 2009 investigation of Siddiqui and Redhwi [26] into the pyrolyses of mixtures of LDPE, HDPE, PP, and PET with PS (e.g., PP+PS) in ratios of 1:1, 1:2, and 1:3 (w/w), in which they report the effects of the plastics on the production of pyrolysis gases at process temperatures of 4”
- Waste Polyolefins to Liquid Fuels via Pyrolysis: Review of Commercial State-of-the-Art and Recent Laboratory Research (2011, unknown): “When PS is present the 24 liquid/wax yields increase since higher liquid yields from polyaromatic plastics are possible 25 [51,8,134].”