In vivo corrosion of four magnesium alloys and the associated bone response.
By F. Witte, V. Kaese, H. Haferkamp, E. Switzer, A. Meyer-Lindenberg, C. Wirth, H. Windhagen. Biomaterials, 2005
2,221 citations recorded by the source corpus.
Subfields: Biomaterials, Biomedical Engineering, Surgery
View Paper: https://www.semanticscholar.org/paper/079b025ab241869cd8fad7f8245ed03aff7642d9
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomaterials
- R. Zeng
- P. Uggowitzer
- G. Dias
- Shaylin Shadanbaz
- Yufeng Zheng
- James F Curtin
- Sankalp Agarwal
- B. Duffy
In Biomedical Engineering
In Surgery
- P. Uggowitzer
- Shaylin Shadanbaz
- R. Singh
- J. Knowles
- M. AlQaysi
- G. Dias
- F. Foroutan
- Chinmaya Mahapatra
Citations in the corpus
- MgZnCa glasses without clinically observable hydrogen evolution for biodegradable implants. (2009, background): “Progress in alloy development, resulting mainly in new compositions and high-purity alloys, has produced an increased corrosion resistance and thus a reduced hydrogen-evolution rat”
- Magnesium alloys for temporary implants in osteosynthesis: in vivo studies of their degradation and interaction with bone. (2012, background): “In this context, numerous studies have been focusing on evaluating the degradation performance of the implant materials and its optimization [3–7].”
- Bioactive glass in tissue engineering (2011, positive): “Biodegradable metals are currently under investigation [33], but their corrosion behavior in vivo remains a key concern.”
- Biodegradable magnesium alloys for orthopaedic applications: A review on corrosion, biocompatibility and surface modifications. (2016, background): “Initially, the rapid formation of H2 gas bubble subcutaneously occurs due to the enriched chloride environment, which can disappear after the initial weeks following surgery [27].”
- Research on an Mg-Zn alloy as a degradable biomaterial. (2010, neutral): “No adverse effects due to these gas bubbles were observed in the rabbits and they disappeared after 6 weeks without any intervention, which is in agreement with the literature [4,6].”
- Calcium phosphate coatings on magnesium alloys for biomedical applications: a review. (2012, positive): “This would also minimize hydrogen production, which has been observed as a (potentially disadvantageous) corrosion byproduct when using this material [29–32].”