Workpiece damping and its effect on delamination damage in drilling thin composite laminates
By E. Capello. 2004
222 citations recorded by the source corpus.
Subfields: Biomedical Engineering, Electrical and Electronic Engineering, Mechanical Engineering
View Paper: https://www.semanticscholar.org/paper/02863c151bc4bf78619102308499008e16293bc4
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Biomedical Engineering
In Electrical and Electronic Engineering
In Mechanical Engineering
Citations in the corpus
- Drilling of polymer matrix composites: A review (2013, background): “When the feed becomes too high, the whole drill point acts as a punch that pierces the laminate.(54) The piercing action result in approximately constant push-out delamination size irrespective to the value of the thrust force (piercing force) (Figure 16).”
- Assessment of delamination in composite materials: A review (2016, background): “This causes delamination at the exit face of the workpiece.(7,8) Push-out mechanism is shown schematically in Figure 2.”
- Effects of special drill bits on drilling-induced delamination of composite materials (2006, background): “There are different approaches from the point geometry to reduce delamination [32,33,37].”