Interpreting hydrogen-induced fracture surfaces in terms of deformation processes: A new approach
By May L. Martin, I. M. Robertson, P. Sofronis. 2011
178 citations recorded by the source corpus.
Subfields: Materials Chemistry, Metals and Alloys
View Paper: https://www.semanticscholar.org/paper/01dd266e1c9ace82f0c2d54a75941955da997976
How researchers see this paper
The researchers whose trusted networks rank it highest, strongest advocate first. Every researcher gets a different order.
In Materials Chemistry
In Metals and Alloys
Citations in the corpus
- Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials (2019, background): “nanometers of the fracture surface, with no visible perturbation on the fracture surface [50].”
- Hydrogen embrittlement controlled by reaction of dislocation with grain boundary in alpha-iron (2018, background): “ted with hydrogeninduced failure (Gerberich, 2012; Robertson et al., 2015; Wang et al., 2016); (iii) how can the experimentally observed quasi-cleavage like fractograph of hydrogen embrittled metals (Martin et al., 2011a; Martin et al., 2011b; Nagao et al., 2012) be explained by the HEDE theory. The”